How to Case Harden Steel
Bone-charcoal color case hardening is heated to the neighborhood of 1300 to 1400°F. Case hardening creates a hard, wear-resistant outer layer over a tougher core. The method works best on suitable low-carbon steel and noncritical parts that can tolerate heat treatment. Process Typical Temperature Best Use Conventional carburizing Use the documented temperature for the carburizing…